Our company adheres to the principle of 'integrity-based, quality-oriented', and has established good long-term cooperative relations with customers at home and abroad. We strive to build ourselves into a manufacturer of casting parts, aluminum alloy casting for certification, aluminum alloy casting for sales management that new and old customers can trust for life.We uphold the attitude of integrity, sincerity and responsibility, optimize the product structure, and provide agents and consumers with more high-quality, reliable and cost-effective Superalloy Casting. We are guided by scientific and technological investment, guaranteed by advanced equipment, excellent quality, and quick after-sales service to win the trust of our customers. Our company continuously strengthens brand strategy, innovation and intellectual property protection strategy, talent and technology strategy and win-win cooperation strategy. 'Technology, quality, service, reputation' as the business philosophy, our company to excellent quality, low price, perfect after-sales service for the purpose. We strive to maintain a leading position in the industry, improve market share and enhance our competitive advantage. Economic efficiency is the goal we pursue, reputation is the lifeblood of enterprise development, and quality is the condition for enterprise survival. We welcome friends from all walks of life at home and abroad to visit our factory and cooperate together. We always regard quality first and service first as our corporate tenet, and continue to provide customers with high-quality services.
  • High Strength Al Alloy Casting
    High Strength Al Alloy Casting

    Dimension: 956×613×274mm. Alloy: ZL401A. Qualification: Mechanical properties as cast reach σb≥241MPa, δ≥1.5%.. Dimensional precision conforms to CT8 of HBG03-86.
    Add to Inquiry
  • Airplane Door
    Airplane Door

    Dimension: 650×350×100mm. Casting section thickness: 2mm. Alloy: D357. Quality: Internal quality conforms to class I of AMS-21180 by X-ray inspection..
    Add to Inquiry
  • Ti Alloy Turbine Impeller
    Ti Alloy Turbine Impeller

    The turbine impeller is made from TC4 titanium alloy. TC4 titanium alloy boasts outstanding comprehensive properties and TC4 parts meet the requirements to be used in harsh environment. The high
    Add to Inquiry
  • Al Alloy Casting
    Al Alloy Casting

    Outer dimension: ∅5200mm*1100. Weight: 5100 kg. Alloy: ZL114A. Casting method: gravity casting.
    Add to Inquiry
  • Alluminum Alloy Casting
    Alluminum Alloy Casting

    Dimension: 956×613×274mm. Alloy: ZL401A. Qualification: Mechanical properties as cast reach σb≥241MPa, δ≥1.5%.. Dimensional precision conforms to CT8 of HBG03-86. Casting Method: Low pressure casting.
    Add to Inquiry
  • Low Pressure Al Alloy Casting
    Low Pressure Al Alloy Casting

    Dimension: 2280×1610×1100mm. Alloy: ZL102. Quality: able to work at 150℃, no leak under 0.5Mpa pressure.. Casting Method: Low pressure casting.
    Add to Inquiry
  • Al Alloy Upper Casing
    Al Alloy Upper Casing

    Weight:54 kg. Alloy:ZAlSi7Mg0.3. Casting method:Low pressure casting. Mechanical properties: Rm≥ 300 MPa, Rp0.2≥240 MPa, A≥ 3%. Dimensional precision: Class CT.
    Add to Inquiry
  • Al Alloy Ring
    Al Alloy Ring

    Outer dimension: φ2780×300 mm. Weight: 1800 kg. Alloy: ZL114A. Casting method: Gravity casting . Dimensional tolerance: Class CT.
    Add to Inquiry
  • Large Al Alloy Casting
    Large Al Alloy Casting

    Dimension: 2280×1610×1100mm. Alloy: ZL102. Quality: able to work at 150℃, no leak under 0.5Mpa pressure.. Casting Method: Low pressure casting.
    Add to Inquiry
  • Upper Casing Aluminum Alloy Casting
    Upper Casing Aluminum Alloy Casting

    Weight: 54 kg. Alloy: ZAlSi7Mg0.3. Casting method: Low pressure casting. Mechanical properties: Rm≥ 300 MPa, Rp0.2≥240 MPa, A≥ 3%. Dimensional precision: Class CT.
    Add to Inquiry
  • Al Alloy Castings
    Al Alloy Castings

    Outer dimension: φ2780×300 mm. Weight: 1800 kg. Alloy: ZL114A. Casting method: Gravity casting. Dimensional tolerance: Class CT.
    Add to Inquiry
  • Super Alloy Casting
    Super Alloy Casting

    The New Technology Research and Development Center of SRIF specializes in R&D of super alloy and special steel precision casting, as well as the production of precision castings.
    Add to Inquiry
Marlo Coleman star star star star star
The delivery speed of the store is very fast. Orders are placed in the morning and goods are delivered in the afternoon. The customer service attitude was also very good, and they were online 24
Brain Bauer star star star star star
We have received the product and are very surprised by the fast logistics and also impressed by the exquisite workmanship of the products produced by your company, hope to continue to cooperate with
Carl Coons star star star star star
Fast delivery, and the price is much more affordable than others!
Kimberly Buhl star star star star star
The biggest difference between your company and other companies is that you are very serious about each customer, you infect us with patience and enthusiasm.
Nicole Roberts star star star star star
We also have a lot of research on this industry, and this cooperation allows us to feel their rich experience, unique insights, and innovative spirit.
John Patterson star star star star star
You are very efficient and you have a positive attitude, how can you not love that?
We continue to improve bearing casting, high pressure casting aluminum alloy quality and reliability indicators to achieve agility, efficiency and standardization of service guarantees. As one of the most professional Superalloy Casting manufacturers and suppliers in China, we're featured by premium investment castings with competitive price. Please rest assured to buy high quality customized Superalloy Casting from our factory. Contact us for quotation.
Contact Us
  • Tel: +86-024-25872276
  • Fax: +86-024-25872276
  • Email: srif@chinasrif.com
  • Add: 17 South Yunfeng Street, Tiexi District, Shenyang P.R. China

(0/10)

clearall