We follow the concept of environmental symbiosis and are committed to the development, production and sales of green aluminum alloy casting for brackets, coating of casting, casting evolution .The pursuit of repair of casting defect excellence is our unswerving goal and our commitment to our customers and society! We warmly welcome domestic and abroad buyers deliver inquiry to us, we now have 24hours doing work team! We adhere to the work policy of respecting labor, talent and creation, and actively shape a good working atmosphere and environment. Our company is dedicated to innovation and excellence in all that we do. We rely on science and technology and modern management to promote the development of our company. We are committed to delivering top-quality products at competitive prices to our customers around the world. We strive to exceed our customers' expectations through unparalleled service and support.
-
High Strength Al Alloy CastingDimension: 956×613×274mm. Alloy: ZL401A. Qualification: Mechanical properties as cast reach σb≥241MPa, δ≥1.5%.. Dimensional precision conforms to CT8 of HBG03-86.Add to Inquiry
-
Airplane DoorDimension: 650×350×100mm. Casting section thickness: 2mm. Alloy: D357. Quality: Internal quality conforms to class I of AMS-21180 by X-ray inspection..Add to Inquiry
-
Monobloc Stainless Steel Pelton RunnerMaterial: ASTM A743 Gr CA6NM, ZG0Cr13Ni4Mo (ZG0Cr13Ni5Mo ZG0Cr16Ni5Mo, etc.) AOD refined stainless steel.. Method: sand casting. Maximum net weight: 8000 kg individual Pelton runner. Delivery state:Add to Inquiry
-
Al Alloy CastingOuter dimension: ∅5200mm*1100. Weight: 5100 kg. Alloy: ZL114A. Casting method: gravity casting.Add to Inquiry
-
Alluminum Alloy CastingDimension: 956×613×274mm. Alloy: ZL401A. Qualification: Mechanical properties as cast reach σb≥241MPa, δ≥1.5%.. Dimensional precision conforms to CT8 of HBG03-86. Casting Method: Low pressure casting.Add to Inquiry
-
Low Pressure Al Alloy CastingDimension: 2280×1610×1100mm. Alloy: ZL102. Quality: able to work at 150℃, no leak under 0.5Mpa pressure.. Casting Method: Low pressure casting.Add to Inquiry
-
Al Alloy Upper CasingWeight:54 kg. Alloy:ZAlSi7Mg0.3. Casting method:Low pressure casting. Mechanical properties: Rm≥ 300 MPa, Rp0.2≥240 MPa, A≥ 3%. Dimensional precision: Class CT.Add to Inquiry
-
Al Alloy RingOuter dimension: φ2780×300 mm. Weight: 1800 kg. Alloy: ZL114A. Casting method: Gravity casting . Dimensional tolerance: Class CT.Add to Inquiry
-
Large Al Alloy CastingDimension: 2280×1610×1100mm. Alloy: ZL102. Quality: able to work at 150℃, no leak under 0.5Mpa pressure.. Casting Method: Low pressure casting.Add to Inquiry
-
Upper Casing Aluminum Alloy CastingWeight: 54 kg. Alloy: ZAlSi7Mg0.3. Casting method: Low pressure casting. Mechanical properties: Rm≥ 300 MPa, Rp0.2≥240 MPa, A≥ 3%. Dimensional precision: Class CT.Add to Inquiry
-
Al Alloy CastingsOuter dimension: φ2780×300 mm. Weight: 1800 kg. Alloy: ZL114A. Casting method: Gravity casting. Dimensional tolerance: Class CT.Add to Inquiry
-
Ti Alloy ValveThis is a titanium alloy valve cast for a ship building company. The outer dimension of the casting is 910 mm× 255 mm× 255 mm, and the wall thickness of the valve is 6mm.Add to Inquiry
The strength of this company is very strong, it quickly helped us complete urgent orders and also met our product customization needs. We recommend it to everyone.
The company has always been realistic. Good product quality, reasonable price and integrity as the fundamental business purposes.
The service was definitely one of the highlights of the store - they were responding to my questions even in the middle of the night. And they alert me when there's an update on the shipment status.
This supplier is indeed more cost-effective.
The company is able to combine market characteristics and introduce products with excellent performance and low price, and the products we received are great and we are very satisfied.
The delivery was very fast, and this order was urgent, but I received the product very quickly, and the workmanship was excellent with naked eyes, which was simply worth the money.
In the past few years, we have cooperated with major domestic aluminum alloy casting for renovations, magnesium alloy casting for performance enhancing use manufacturers as well as state-owned enterprises, private enterprises and other end customers, and have been well received. As one of the most professional repair of casting defect manufacturers and suppliers in China, we're featured by premium investment castings with competitive price. Please rest assured to buy high quality customized repair of casting defect from our factory. Contact us for quotation.
Categories
Latest Products
Contact Us
- Tel: +86-024-25872276
- Fax: +86-024-25872276
- Email: srif@chinasrif.com
- Add: 17 South Yunfeng Street, Tiexi District, Shenyang P.R. China