China customization service for superalloy casting Manufacturers Factory Suppliers

With advanced technologies and facilities, strict good quality manage, reasonable rate, superior assistance and close co-operation with shoppers, we have been devoted to supplying the very best price for grinding of superalloy casting, cloud computing application of superalloy casting, automation application of superalloy casting .We provide you with the best quality customization service for superalloy casting in the market at any time with the most comprehensive service and professional knowledge brought by the accumulation of long-term experience. Our team of experts brings a wealth of knowledge and experience to every project we undertake. Our team is committed to delivering high-quality products and services at competitive prices. We are market-oriented and user-oriented, closely follow the market demand, closely follow the industry trend. We have gradually matured in the baptism of the market for many years and have emerged in the industry. We take the initiative to adapt to the new normal of environmental protection, strengthen the environmental protection responsibility system, and keep the bottom line of environmental protection.
  • Super Alloy Casting Pump Body
    Super Alloy Casting Pump Body

    Our main products are impellers, blades, shells, shaped castings customized for aviation, aerospace, metallurgy, chemical engineering, ship building, power generation and other fields.
    Add to Inquiry
  • Mg Alloy Casting
    Mg Alloy Casting

    Dimension: Φ700×500mm. Alloy: ZM5. Quality: Internal quality conforms to class Ⅱ of HB965-84 by X-ray inspection.. Casting Method: Low pressure casting.
    Add to Inquiry
  • Ti Alloy Impeller
    Ti Alloy Impeller

    This titanium impeller casting is widely used in pumps and valves for the chemical industry. The material of the product is TA2 titanium alloy with common mechanical properties, excellent erosion
    Add to Inquiry
  • Ti Alloy Turbine Impeller
    Ti Alloy Turbine Impeller

    The turbine impeller is made from TC4 titanium alloy. TC4 titanium alloy boasts outstanding comprehensive properties and TC4 parts meet the requirements to be used in harsh environment. The high
    Add to Inquiry
  • Stainless Steel Blade
    Stainless Steel Blade

    The stainless steel blade for Francis runner, ready to be assembled, is produced with sand casting techniques. Individual blades weighing not more than 6000kg can be provided. Axial flow blades
    Add to Inquiry
  • Monobloc Stainless Steel Pelton Runner
    Monobloc Stainless Steel Pelton Runner

    Material: ASTM A743 Gr CA6NM, ZG0Cr13Ni4Mo (ZG0Cr13Ni5Mo ZG0Cr16Ni5Mo, etc.) AOD refined stainless steel.. Method: sand casting. Maximum net weight: 8000 kg individual Pelton runner. Delivery state:
    Add to Inquiry
  • Al Alloy Upper Casing
    Al Alloy Upper Casing

    Weight:54 kg. Alloy:ZAlSi7Mg0.3. Casting method:Low pressure casting. Mechanical properties: Rm≥ 300 MPa, Rp0.2≥240 MPa, A≥ 3%. Dimensional precision: Class CT.
    Add to Inquiry
  • High Strength Al Alloy Casting
    High Strength Al Alloy Casting

    Dimension: 956×613×274mm. Alloy: ZL401A. Qualification: Mechanical properties as cast reach σb≥241MPa, δ≥1.5%.. Dimensional precision conforms to CT8 of HBG03-86.
    Add to Inquiry
  • Large Al Alloy Casting
    Large Al Alloy Casting

    Dimension: 2280×1610×1100mm. Alloy: ZL102. Quality: able to work at 150℃, no leak under 0.5Mpa pressure.. Casting Method: Low pressure casting.
    Add to Inquiry
  • Al Alloy Castings
    Al Alloy Castings

    Outer dimension: φ2780×300 mm. Weight: 1800 kg. Alloy: ZL114A. Casting method: Gravity casting. Dimensional tolerance: Class CT.
    Add to Inquiry
  • Stainless Steel Francis Runner
    Stainless Steel Francis Runner

    The crown, the band and the blades are sand cast and machined separately before being integrated into a whole by welding. We are capable of manufacturing crowns, bands or blades weighing not more
    Add to Inquiry
  • Super Alloy Casting
    Super Alloy Casting

    The New Technology Research and Development Center of SRIF specializes in R&D of super alloy and special steel precision casting, as well as the production of precision castings.
    Add to Inquiry
Donna Watson star star star star star
We like this product. On the whole, it is the best, and the packaging during transportation is great.
Kathy Quintana star star star star star
This is a very welcoming vendor that answered all my questions quickly and I hope we can continue to work together next time.
Samuel Browne star star star star star
The factory is like the ivy, the product is like the gourd on the vine; Only good melons can sell at a good price. The factory's efficiency depends on it.
Patricia Delano star star star star star
Our boss is impressed by the professionalism of your employees and the fact that you have been smiling and serving your customers is very satisfying.
Natalia Hammond star star star star star
Unpacked, they have enough products, the quality is the same, there is no defect or broken, customers love it.
Ashley Rodriguez star star star star star
You are a hundred-year enterprise, we wish you better and better development!
We cooperate sincerely with multinational companies, and our aluminum alloy casting for competitive advantage, metal casting machinery and manufacturing technology are in line with the world. As one of the most professional customization service for superalloy casting manufacturers and suppliers in China, we're featured by premium investment castings with competitive price. Please rest assured to buy high quality customized customization service for superalloy casting from our factory. Contact us for quotation.
Contact Us
  • Tel: +86-024-25872276
  • Fax: +86-024-25872276
  • Email: srif@chinasrif.com
  • Add: 17 South Yunfeng Street, Tiexi District, Shenyang P.R. China

(0/10)