China casting defect Manufacturers Factory Suppliers
We give full play to the reasonable layout of the factory and the superiority of advanced technology and equipment to produce high-performance recyclable casting, machining of casting, casting customer .As a newly emerging manufacturer of high-end casting defect, we stick to the core values of forge ahead, mutual benefit, efficient collaboration, and craftsmanship as our guide. We will focus on the five major development concepts of innovation, coordination, green, openness and sharing, and adhere to the direction of market-oriented reform. Our success comes from our people, with whom we work in a safe and satisfying environment. We choose to treat each other with trust and respect and to maintain a healthy balance between work and family life. We can provide our customers with best products and best service, and are desired to cooperate with you for common development. With brand-new design concepts, first-class quality, professional workmanship, we have a broad market and a good reputation! We have strong competitiveness in the same industry and we can provide users with protection and maximum economic benefits.
-
Al Alloy CastingOuter dimension: ∅5200mm*1100. Weight: 5100 kg. Alloy: ZL114A. Casting method: gravity casting.Add to Inquiry
-
Airplane DoorDimension: 650×350×100mm. Casting section thickness: 2mm. Alloy: D357. Quality: Internal quality conforms to class I of AMS-21180 by X-ray inspection..Add to Inquiry
-
Stainless Steel BladeThe stainless steel blade for Francis runner, ready to be assembled, is produced with sand casting techniques. Individual blades weighing not more than 6000kg can be provided. Axial flow bladesAdd to Inquiry
-
Alluminum Alloy CastingDimension: 956×613×274mm. Alloy: ZL401A. Qualification: Mechanical properties as cast reach σb≥241MPa, δ≥1.5%.. Dimensional precision conforms to CT8 of HBG03-86. Casting Method: Low pressure casting.Add to Inquiry
-
Low Pressure Al Alloy CastingDimension: 2280×1610×1100mm. Alloy: ZL102. Quality: able to work at 150℃, no leak under 0.5Mpa pressure.. Casting Method: Low pressure casting.Add to Inquiry
-
Al Alloy Upper CasingWeight:54 kg. Alloy:ZAlSi7Mg0.3. Casting method:Low pressure casting. Mechanical properties: Rm≥ 300 MPa, Rp0.2≥240 MPa, A≥ 3%. Dimensional precision: Class CT.Add to Inquiry
-
Al Alloy RingOuter dimension: φ2780×300 mm. Weight: 1800 kg. Alloy: ZL114A. Casting method: Gravity casting . Dimensional tolerance: Class CT.Add to Inquiry
-
High Strength Al Alloy CastingDimension: 956×613×274mm. Alloy: ZL401A. Qualification: Mechanical properties as cast reach σb≥241MPa, δ≥1.5%.. Dimensional precision conforms to CT8 of HBG03-86.Add to Inquiry
-
Large Al Alloy CastingDimension: 2280×1610×1100mm. Alloy: ZL102. Quality: able to work at 150℃, no leak under 0.5Mpa pressure.. Casting Method: Low pressure casting.Add to Inquiry
-
Upper Casing Aluminum Alloy CastingWeight: 54 kg. Alloy: ZAlSi7Mg0.3. Casting method: Low pressure casting. Mechanical properties: Rm≥ 300 MPa, Rp0.2≥240 MPa, A≥ 3%. Dimensional precision: Class CT.Add to Inquiry
-
Al Alloy CastingsOuter dimension: φ2780×300 mm. Weight: 1800 kg. Alloy: ZL114A. Casting method: Gravity casting. Dimensional tolerance: Class CT.Add to Inquiry
-
Large Ti Alloy CastingThe turbine impeller is made from Ti-6Al-4V titanium alloy. Ti-6Al-4V titanium alloy boasts outstanding comprehensive properties and Ti-6Al-4V parts meet the requirements to be used in harshAdd to Inquiry
The quality of these items is very good to me and I will recommend them to more people!
The company's technicians are patient, not perfunctory, and have taken the trouble to solve all our problems.
This supplier is very honest and I strongly support it.
This time, we bought the customized products, which are the best among all the customized products. We are very satisfied with the company's service and hope that more people will cooperate with you.
The product is very good and the service attitude is also very good!
Our order leader is very approachable and enhances our overall cooperation experience. Their products also met our expectations in every way.
The core technology and characteristics of our purpose of casting, magnesium alloy casting for shipments are high efficiency and energy saving, and we are committed to become the leading domestic and international advanced level. As one of the most professional casting defect manufacturers and suppliers in China, we're featured by premium investment castings with competitive price. Please rest assured to buy high quality customized casting defect from our factory. Contact us for quotation.